We know your urgency. Call us: +91 98554 45055
Vishwakarma Technical Services (VTS)
Pune, India · RLA & NDT specialists
Home / Services / Ultrasonic Thickness Inspection
NDT / NDE and Inspection

Ultrasonic Thickness Inspection (UTM)

Remaining wall thickness and hidden corrosion on tubes, pipes and vessels.

Service overview

Ultrasonic thickness measurement finds the remaining wall thickness of a component from one side. Readings taken over time show corrosion and erosion trends and help decide when to repair or replace.

Purpose and industrial applications

  • Boiler tube and header wall-loss surveys
  • Pressure vessel and tank thickness mapping
  • Input data for remaining life assessment

Components and materials

  • Boiler, superheater and economiser tubes
  • Headers, shells, dished ends and nozzles
  • Pipes, heaters and storage vessels

Inspection methods and equipment

  • Portable ultrasonic thickness gauge
  • Step gauge for calibration on the job
  • Probes suited to the thickness range and temperature

See our equipment

Typical procedure

  1. Define the grid or locations to be measured
  2. Clean the surface and apply couplant
  3. Calibrate on a step gauge
  4. Record readings at each location
  5. Compare with design and minimum required thickness

Applicable codes and standards

Readings are evaluated against design thickness, minimum required thickness and the client or statutory criteria for the equipment.

The applicable standard depends on the equipment, material, service conditions, statutory requirements and the approved scope of work.

Deliverables and reporting

  • Thickness readings in tabulated form
  • Location sketch or grid map
  • Comparison with minimum required thickness
  • Wall-loss trend where earlier readings exist

Scope limitations and site requirements

  • Surface condition and scale affect accuracy
  • High surface temperature needs suitable probes and couplant
  • Readings show thickness at the points measured only

Frequently asked questions

How often should thickness be checked?
It depends on the corrosion rate, the service and the equipment history. We help plan an interval, see Inspection Planning.
Does it find internal corrosion?
It shows the remaining thickness where corrosion has reduced it. It does not image the whole internal surface.
ISO 9001:2015Certified quality management
On-time complianceESIC, PF and MLWF awards
Safety firstPPE and LOTO kits in use
60+ page reportsDetailed documentation per project
IBR-certified weldersFor boiler pressure parts

Planning a shutdown or facing a breakdown?

We know your urgency. Tell us the problem and we will plan the right testing.

Send an enquiry